Re: [NTLK] eMate disassembly - do I *have* to de-solder?/my emate just came

From: Woody Smith (woody_at_bitstream.net)
Date: Thu May 27 2004 - 09:50:32 PDT


David
Thanks for the info.
Woody
On Thursday, May 27, 2004, at 09:15 AM, Humphreys, David wrote:
>
> I see. But...
>
> 96/4 Tin/Silver MP = 460F
>
> 60/40 Tin/Lead MP = 430F
>
> 63/37 Tin/Lead eutectic MP = 349F
>

snip

> Now you can use Tin/Silver solder but it is not the best for
> electronic board work. It is better as a hobbyist solder
> for model railroad tracks due to the superior strength of the joints
> it makes.
>
> Regards,
>
> PCBman

-- 